Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 154 MPa | 22400 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM3 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedAppearance: RedInformation provi.. |