Polymer Property : Tensile Strength, Yield = 220200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1518 MPa
220200 psi
Hardened 1900°F, Tempered 550°F
ATI Allegheny Ludlum 440A Martensitic Stainless Steel
Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for..
Tensile Strength, Yield 1518 MPa

@Strain 0.200 %
220200 psi

@Strain 0.200 %
typical
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 288°C Temper
Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle..