Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 15.00 MPa | 2176 psi | At 50 mm/min; ISO 527-2 |
Borealis Daplen™ EG203AE Polypropylene Compound Elastomer and Mineral Modified Daplen EG203AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EG203AE is a material with excellent impact /stiffness ratio. Thanks to its low .. |
|||
Tensile Strength, Yield | 15.00 MPa | 2176 psi | Change in tensile strength after 240 hours at 239°F; ASTM D638 |
Teknor Apex Sinvicomp SIH 6508A Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Good Stiffness Uses: Wire and Cable Applications Wire Types: V-75 Agency Ratings: AS 3147-1992 Forms: Pellets Processing Method: ExtrusionInformation Provided by.. |
|||
Tensile Strength, Yield | >= 15.00 MPa | >= 2176 psi | 2 in/min; LAB032 |
ExxonMobil Mytex™ AN17K-01 Rubber modified polypropylene for automotive interior applications.Information provided by ExxonMobil Chemical |