Tensile Strength, Yield 1470 MPa
213000 psi
50 HRC, Round bar 1" diameter, Hardened in oil from 1880°F and tempered twice
EDRO #8 Premium 420 Stainless Mold Steel
EDRO #8™ is a chromium-alloyed stainless tool steel with the following properties: excellent corrosion resistance, superior polishability, good wear resistance, good machinability, and stability in..