Mechanical Properties Metric English Comments
Tensile Strength, Yield 2120 MPa

@Temperature 23.0 °C
307000 psi

@Temperature 73.4 °F
Hexcel® HexPly® 954-3A Curing Cyanate Resin, M60J Fiber
Information provided by HexCel
Tensile Strength, Yield 2120 MPa
307000 psi
Elgiloy® Co-Cr-Ni Alloy, Strip, 85% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High ..