Polymer Property : Tensile Strength, Yield = 21.89 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.89 MPa
3175 psi
ASTM D-638
Axiall 10850 Wire & Cable Flexible PVC
Non-metallic conduit. 3/4" and smaller.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 21.89 MPa
3175 psi
ASTM D-638
Axiall 4470 Flexible PVC
High speed ultrathinwall automotive harness wire per SAE J1128.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.