Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 21.39 MPa | 3103 psi | at 500 mm; ASTM D638 |
ExxonMobil HD 6510 Injection Molding Resin
(discontinued **) HD 6510 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a wide ra.. |
|||
Tensile Strength, Yield | 21.39 MPa | 3103 psi | at 500 mm; ASTM D638 |
ExxonMobil HD 6510.17 Injection Molding Resin
(discontinued **) HD 6510 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a wide ra.. |