Tensile Strength, Yield 105 - 208 MPa
15200 - 30200 psi
Average value: 157 MPa Grade Count:11
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..