Tensile Strength, Yield 1091 - 1416 MPa
158200 - 205400 psi
Latrobe Magnadieâ„¢ Modified H-13 Hot Work Die Steel
MAGNADIE is an AOD refined, air hardenable 5% chromium die steel. It is a good choice for both hot and cold work applications. Magnadie steel possesses improved toughness as compared to standard H-..