Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 141 MPa | 20400 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 GF30 FR-N 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame Retardant and Halogen FreeInformation provided by TP Composites, Inc. |