Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 13.95 MPa
2023 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 7182E Fluorocarbon-Elastomer
Formulated AFLAS® high-temperature "sour" oil & gas service. Excellent acid and base resistance.Information provided by Seals Eastern, Inc.