Mechanical Properties Metric English Comments
Tensile Strength, Yield 13.9 MPa
2020 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR DBPH-50
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tensile Strength, Yield 13.9 MPa
2020 psi
20 in/min; ASTM D638
Teknor Apex Sinvicomp SMG 6500 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Toys Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Tensile Strength, Yield 13.9 MPa
2020 psi
ASTM D412
Vicone High Performance Rubber VicoSil™ C306E-GR High Performance Silicone Rubber
Information provided by Vicone
Tensile Strength, Yield 13.9 MPa
2020 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR DBPH-50
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..