Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.14 MPa | 311 psi | at 200%, as molded- 10 minutes at 116°C |
Multibase SILASTIC® Q7-4750 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 2.14 MPa | 310 psi | ASTM D412 |
Polymax® Maxelast® C4907 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Strength, Yield | 2.14 MPa | 310 psi | 200%, post cured- 8 hours at 177°C; ASTM D412 |
Multibase C6-135 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 2.14 MPa | 310 psi | AVG Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7075 Ethylene-Propylene Rubber General service EPDM.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 2.14 MPa | 311 psi | at 150% Elongation, maximum |
Dow Corning SILASTIC® LS 4-9060 FLUOROSILICONE RUBBER 60 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning |
|||
Tensile Strength, Yield | 2.14 MPa | 310 psi | at 100%; ASTM D412 |
Multibase Multi-Flex® A 6202 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |