Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.11 MPa | 306 psi | 200%, post cured- 4 hours at 177°C; ASTM D412 |
Multibase C6-135 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 2.11 MPa | 306 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 7145 Fluorocarbon-Elastomer FKM specially for oil & gas service.Information provided by Seals Eastern, Inc. |