Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1360 MPa | 197000 psi | |
Kinetics MIM 4605 Low Alloy Steel (Austempered) Low alloy steel, carbon, nickel, molybdenum. A multi-purpose, economical material that offers various strength, hardness, and wear resistance properties depending if it is heat treated and the heat .. |
|||
Tensile Strength, Yield | 1360 MPa | 197000 psi | Hardened 1900°F, Tempered 550°F |
ATI Allegheny Ludlum 425 Mod Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Yield | 1360 MPa @Strain 0.200 % |
197000 psi @Strain 0.200 % |
typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 288°C Temper Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai.. |