Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 1.36 MPa | >= 197 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 5053 Ethylene-Propylene Rubber General service EPDM.Information provided by Seals Eastern, Inc. |