Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 13.22 MPa | 1917 psi | Change in tensile strength after 168 hours at 212°F; ASTM D638 |
Teknor Apex Sinvicomp SIM 4019 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 13.22 MPa | 1917 psi | Change in tensile strength after 504 hours at 250°C; ASTM D638 |
Teknor Apex Sinvicomp SIH 5008 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Good Stiffness Uses: Electronic Insulation; Wire and Cable Applications Wire Types: Y17 Agency Ratings: BS 6746; JIS 6723; VDE 0207 Forms: Pellets Processing Met.. |