Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 19.82 MPa | 2875 psi | ASTM D-638 |
Axiall 19930 Wire & Cable Flexible PVC THHN-THWN circuit sizes. Best suited for 105°C; 1/64 (18 AWG and larger). Rated VW-1. CSA approved TWN75, TEW, AWM IA, FT1 constructions. UL recognized for TW, THW, THWN, THHN. Oil resistant I.. |