Polymer Property : Tensile Strength, Yield = 1850 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1850 MPa

@Temperature 23.0 °C
268000 psi

@Temperature 73.4 °F
Assab Steels HOTVAR Hot Work Steel
HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue..