Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 12.75 MPa | 1849 psi | -15% change after 168 hours @ 70°C; ASTM D412 |
Precision Polymer Engineering R50D Natural Rubber Natural Rubber, 45-55 °IRHD. Formulated to Defence Standard 93-30, Type QX, Grade 50 (NRQX50).Applications: Natural rubber offers low compression set, high tensile strength, high resilience and ex.. |
|||
Tensile Strength, Yield | 12.75 MPa | 1849 psi | -15% change after 72 hours @ 250°C; ASTM D412 |
Precision Polymer Engineering V80D Fluoroelastomer Compound Fluoroelastomer Rubber, 75-84 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Meets Aerospace Specifications DTD5612A and DTD5543B Grade 80.Applications: Mouldings which are requ.. |