Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 12.7 MPa | 1840 psi | ASTM D412 |
Precision Polymer Engineering V90B Fluoroelastomer Compound Fluoroelastomer Rubber, 85-95 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M5HK910, A1-11, B38, EF31, EO78, F15, Z1. Where Z1 = compression s.. |
|||
Tensile Strength, Yield | 12.7 MPa | 1840 psi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato.. |
|||
Tensile Strength, Yield | 12.7 MPa | 1840 psi | after aging 1 week @ 135°C; ASTM D638 |
Trelleborg Horda Cable E8502 Strippable Semiconductive Shielding E8502 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8502 meets the requirements as bel.. |
|||
Tensile Strength, Yield | 12.7 MPa | 1840 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3890E Thermoplastic Elastomer - SBC
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |