Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 12.5 MPa | 1820 psi | ASTM D412 |
Polymax® Maxelast® P2885 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 12.5 MPa | 1820 psi | ASTM D412-97 |
Saint-Gobain Tygon® F-4040-A Fuel and Lubricant Tubing Formulation Description: Tygon® F-4040-A: A consistent performer lot after lot, Tygon® Fuel and Lubricant Tubing is the most requested fuel and lubricant tubing for a variety of applications -- from sma.. |
|||
Tensile Strength, Yield | 12.5 MPa | 1820 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SFC 7500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Foamable Uses: Footwear Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |