Mechanical Properties Metric English Comments
Tensile Strength, Yield 1240 MPa
180000 psi
Kinetics MIM 440C Stainless Steel
Martensitic stainless steel. Excellent strength, hardness, and wear resistance while offering some corrosion resistance. Magnetic. Often used for automotive, cutlery, industrial equipment, power han..
Tensile Strength, Yield 1240 - 1520 MPa
180000 - 220000 psi
Materion Beryllium Copper Alloy 25 Wire; HT (TH04) Temper; 1.3-2.0 mm Diameter (UNS C17200)
Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it..
Tensile Strength, Yield 1240 - 1520 MPa
180000 - 220000 psi
Materion Beryllium Copper Alloy M25 Wire; HT (TH04) Temper; 1.3-2.0 mm Diameter (UNS C17300)
Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it..
Tensile Strength, Yield 1241 MPa
180000 psi
Latrobe Lescalloy® HY-180 VIM-VAR ; .375 - 2 thickness High Strength Alloy Steel
LESCALLOY HY-180 VIM-VAR steel is a high strength alloy steel with superior toughness. It is double vacuum melted (VIM-VAR…vacuum induction melted followed by vacuum arc remelting) to provide s..
Tensile Strength, Yield 1240 MPa
180000 psi
ASTM D3039
Greene Tweed Orthetek® RP Polyketone, Random Carbon Fiber
Greene Tweed offers precision-molded thermoplastic components made form out high-performance Orthtek® composite materials for a variety of demanding medical device applications. Orthtek RP is id..
Tensile Strength, Yield 1240 MPa
180000 psi
Wingate Alloys Winco-Tuf 50 Ultra High Strength Alloy Wear Plate
Winco-Tuf 50 quenched and tempered, high alloy steel is intended specifically for applications requiring a high degree of abrasion and wear resistance.Used by industries such as mining, forestry, qu..
Tensile Strength, Yield 1241 MPa

@Strain 0.200 %,
Temperature 371 °C
180000 psi

@Strain 0.200 %,
Temperature 700 °F
Carpenter Custom 455® Stainless Steel, Condition H900 (Age Hardened 482°C)
Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope..
Tensile Strength, Yield 1240 MPa

@Strain 0.200 %
180000 psi

@Strain 0.200 %
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 75% Cold Work
The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co..
Tensile Strength, Yield 1241 MPa
180000 psi
HP Alloys Alloy 718, 30% Cold Worked
30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Tensile Strength, Yield >= 1241 MPa

@Strain 0.200 %
>= 180000 psi

@Strain 0.200 %
HP Alloys Nitronic® 50 Austenitic Stainless, Level 5 Cold Worked
Cold Worked applies to tensile values and are for 0.25 to 1.5 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resis..
Tensile Strength, Yield >= 1241 MPa

@Strain 0.200 %
>= 180000 psi

@Strain 0.200 %
HP Alloys Nitronic® 60 Austenitic Stainless, Level 5 Cold Worked
Level 5 Cold Worked applies to tensile properties of 0.25 to 1.5 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was orig..