Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 0.124 MPa | >= 18.0 psi | ASTM D638 |
Buckeye Polymers BP FLEX D7030 BLK Thermoplastic Elastomer TPV Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |