Mechanical Properties Metric English Comments
Tensile Strength, Yield 121 MPa
17600 psi
ASTM D638
Techmer ES Luriblend® PA6/6 GF30 X 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and He..
Tensile Strength, Yield 122 MPa
17600 psi
ASTM D638
Cheng Yu Plastic A706G15 SAN, 15% Glass Fiber