Polymer Property : Tensile Strength, Yield = 1752 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 12.08 MPa
1752 psi
-20% change after 72 hours @ 250°C; ASTM D412
Precision Polymer Engineering V70B Fluoroelastomer Compound
Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene.Applications: Excellent resistance to oils, fuels and hydraulic fluids at high temperature.