Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1034 - 1207 MPa | 150000 - 175100 psi | |
Materion Beryllium Nickel Strip - Alloy 360 MH6, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |