Polymer Property : Tensile Strength, Yield = 174900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 1206 MPa
>= 174900 psi
Materion Beryllium Nickel Strip - Alloy 360 1/4 Hard, 2.5 hr at 950°F
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 2.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation..