Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1195 MPa @Strain 0.200 % |
173300 psi @Strain 0.200 % |
|
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |