Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1730 MPa @Strain 0.200 % |
251000 psi @Strain 0.200 % |
|
QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications Description: Ferrium® M54™ is an ultra high-strength steel for structural applications. Ferrium® M54™ was designed to provide mechanical properties equal to, or better than ultrahigh-strength st.. |
|||
Tensile Strength, Yield | 1730 MPa @Strain 0.200 % |
251000 psi @Strain 0.200 % |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 45% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |