Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 172.4 MPa @Temperature 538 °C |
25000 psi @Temperature 1000 °F |
|
ATI Allegheny Ludlum Stainless Steel 334 (UNS S33400) Allegheny Ludlum Type 334 is a titanium- and aluminum-bearing austenitic stainless steel offering superior elevated temperature scaling resistance compared to the conventional chromium-nickel stainl.. |