Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 17.42 MPa | 2526 psi | ASTM D-638 |
Axiall 38941 Coax & Telecom Flexible PVC Aerial drop parallel telecom jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |