Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 930 - 1140 MPa | 135000 - 165000 psi | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; HT (TH04) Temper; over 25 to 51 mm Thickness (UNS C17000) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Yield | 930 - 1140 MPa | 135000 - 165000 psi | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; HT (TH04) Temper; over 9.5 to 25 mm Thickness (UNS C17000) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Yield | 930 - 1140 MPa | 135000 - 165000 psi | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; HT (TH04) Temper; up to 9.5 mm Thickness (UNS C17000) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |