Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1650 MPa | 239000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 40% Cold Reduction, Heat Treated Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi.. |
|||
Tensile Strength, Yield | 1650 MPa | 239000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 65% Cold Reduction The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f.. |