Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1621 MPa @Strain 0.200 % |
235100 psi @Strain 0.200 % |
|
ATI Allvac® VascoMax® T-250 Specialty Steel, Heat Treatment: 816°C (1500°F) + Age Data provided by Allvac.Applications: Missile components, tooling and other applications requiring good toughness with high strength. Jet engine shafts. |