Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.65 MPa
2415 psi
-10% change after 72 hours @ 250°C; ASTM D412
Precision Polymer Engineering Perlast® G81T Perfluoroelastomer
A special black perfluoroelastomer compound with PTFE blended for improved mechanical performance. Excellent steam resistance and mechanical properties. Extremely low outgassing properties. Applica..