Polymer Property : Tensile Strength, Yield = 16.40 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.40 MPa
2379 psi
2"/min; ASTM D638
ICO Polymers ICORENEâ„¢ 110-1016 LMDPE Rotational Molding Resin
Description: ICORENE 110-1016 polyethylene developed for use in rotational molding. This is a very fast processing material that quickly molds out to offer low surface porosity and good overall pro..