Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 16.1 MPa | 2340 psi | ASTM D412 |
Precision Polymer Engineering Perlast® G70K Perfluoroelastomer Special white compound with wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Recommended f.. |
|||
Tensile Strength, Yield | 16.1 MPa | 2330 psi | 100%; ASTM D412 |
Teknor Apex MF 141 Polyvinyl Chloride, Flexible Film Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsAppearance-ClearInformation provided by Teknor Apex Company |