Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.04 MPa | 151 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 7027 Butyl and Halobutyl Rubber General purpose Chlorobutyl; High dampingInformation provided by Seals Eastern, Inc. |