Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 15.14 MPa | 2195 psi | 6% change after 168 hours @ 70°C; ASTM D412 |
Precision Polymer Engineering C70C Chloroprene Rubber Chloroprene Rubber, 66-75 °IRHDApplications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum based oils, ozone and weather. Widely used for sealing.. |