Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 98.6 MPa | 14300 psi | |
COI Ceramics Sylramic™ S400 Silicon Carbide Ceramic Matrix Composite, Carbon Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crysta.. |