Polymer Property : Tensile Strength, Yield = 1410 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1410 MPa
204000 psi
International Mold Steel Premium H13 Hot Work Die and Mold Steel
Description: International Mold Steel's Premium H-13 is a chromium-based, hot work die and plastic mold steel designed for increased production rates and longer tool life. It meets the restricti..