Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 14.66 MPa | 2126 psi | AVG Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7182A Fluorocarbon-Elastomer Formulated AFLAS® high-temperature, high-pressure "sour" oil & gas service. Resistant to extrusion. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |