Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 14.4 MPa | 2090 psi | -20% change after 70 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering N70Z Nitrile Rubber Carboxylated Nitrile Butadiene Rubber (XNBR), 65-75 °IRHD. Terpolymer of acrylonitrile, butadiene and methacrylic acid.Applications: Carboxylated Nitrile (XNBR) offers much higher modulus, increas.. |
|||
Tensile Strength, Yield | 14.4 MPa | 2090 psi | ASTM D638 |
NOVA Chemicals Sclair® 8306 UV8D, 8306G UV8D MDPE Rotational Molding Resin
(discontinued **) Features: Balanced combination of toughness, ESCR and processability.Applications: General purpose.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 14.4 MPa | 2090 psi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 10.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
Tensile Strength, Yield | 14.4 MPa | 2090 psi | ASTM D-638 |
Axiall 419-90D Coax & Telecom Flexible PVC 419-90D is a highly flame retardant jacket originally designed for CSA FT-4 type CATV applications and has good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axi.. |
|||
Tensile Strength, Yield | 14.4 - 22.1 MPa | 2090 - 3200 psi | Average value: 18.8 MPa Grade Count:33 |
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu.. |
|||
Tensile Strength, Yield | 14.4 MPa | 2090 psi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 10.0 PHR Wacker HDK N20 Filler Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |