Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 14.31 MPa | 2075 psi | AVG Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7182X Fluorocarbon-Elastomer Formulated AFLAS®. Ultra-low compressive stress relaxation for alkaline, high-temperature service.Information provided by Seals Eastern, Inc. |