Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 14.24 MPa | 2065 psi | -11% change after 72 hours @ 250°C; ASTM D412 |
Precision Polymer Engineering Perlast® G60T Perfluoroelastomer A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: This grade is particularly suited to static ap.. |