Polymer Property : Tensile Strength, Yield = 139000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 960 - 1210 MPa
139000 - 175000 psi
Materion Beryllium Copper Alloy 25 Strip; AT (TF00) Temper (UNS C17200)
Treatment required for max strength: 3 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6..
Tensile Strength, Yield >= 960 MPa

@Strain 0.200 %
>= 139000 psi

@Strain 0.200 %
Industeel SUPERELSO® 960 HLE Steel for Welded and Weight-Saving Structures
Description: SUPERELSO® 960 is quenched and tempered steel for structure with higher strength. Thanks to a minimum yield strength of 960 N/mm² (140 KSI), SUPERELSO® 960 enables to make weig..
Tensile Strength, Yield 960 MPa

@Strain 0.200 %
139000 psi

@Strain 0.200 %
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Tensile Strength, Yield 958 MPa

@Strain 0.200 %,
Temperature 21.1 °C
139000 psi

@Strain 0.200 %,
Temperature 70.0 °F
Latrobe Lescalloy® 6305 VAC-ARC ; High Strength Alloy Steel
LESCALLOY 6305 VAC-ARC steel is a modified 4140 steel with higher molybdenum and a vanadium addition. The alloy steel is generally used in the 160/180,000 psi tensile strength range obtained with a..
Tensile Strength, Yield 958 MPa

@Strain 0.200 %,
Thickness 50.8 mm
139000 psi

@Strain 0.200 %,
Thickness 2.00 in
Latrobe Lescalloy® 6305 VAC-ARC ; High Strength Alloy Steel
LESCALLOY 6305 VAC-ARC steel is a modified 4140 steel with higher molybdenum and a vanadium addition. The alloy steel is generally used in the 160/180,000 psi tensile strength range obtained with a..
Tensile Strength, Yield >= 960 MPa

@Thickness 50.0 mm
>= 139000 psi

@Thickness 1.97 in
ThyssenKrupp XABO® 960 Structural Steel
This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli..
Tensile Strength, Yield 960 MPa

@Strain 0.200 %
139000 psi

@Strain 0.200 %
Typical
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Annealed Sheet/Plate & Billet/Bar
Low Cost, Multipurpose Alloy. Tensile property data below for Annealed Sheet/Plate & Billet/Bar.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but wit..