Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.549 MPa | 1385 psi | ASTM D-638 |
Axiall 8778 Moldings & Extrusions Flexible PVC A general purpose compound recommended for extrusion and molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |