Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 1356 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.349 MPa
1356 psi
60% Retention; Aged 18 hrs at 121°C in Vegetable oil.(ASTM D471)
Teknor Apex ELEXAR® EL 8421 Thermoplastic Elastomer
Information provided by Teknor Apex Company