Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.136 MPa
1325 psi
@100% Elongation; ASTM D1414
Greene Tweed FLUORAZ® 797 Fluoroelastomer, FEPM
Greene, Tweed`s Fluoraz® functions effortlessly in a variety of challenging process environments. Fluoraz performs well in aggressive chemicals where ultrapure materials are not required. Known f..
Tensile Strength, Yield 9.136 MPa
1325 psi
ASTM D412
ACC EP EF EPI Engineered Polymers Extra Flex Polyurea
EP EF, Extra Flex Polyurea, “Powered by Reactamine® Technology, is a two component 100% solid Polyurea, with superior performance in industrial applications. EP EF displays extremely fast cure tim..
Tensile Strength, Yield 9.136 MPa
1325 psi
ASTM D412
ACC SMP™ EP EF SP EPI Engineered Polymers Extra Flex with Silicone
EP EF SP, “Powered by Reactamine® Technology”, is a two component 100% solid Silicone Polyurea with superior performance in industrial applications. EP EF SP displays extremely fast cure times wi..